Views: 0 Author: TOPBOLT technical team Publish Time: 2026-11-20 Origin: Site
Many warehouses place A325 bolts directly on the floor without pallets, and humidity control is missing. As carbon steel high-strength fasteners, A325 bolts are prone to rust in humid environments. North American project inspectors have strict acceptance standards for surface rust, and rust formed during storage often leads to rejection.
Some A325 bolts come with factory pre-coated lubrication, designed to stabilize tightening torque and consistent preload. If stored together with cutting oil, dust and metal debris, the original lubricant layer will be contaminated or scratched. Damaged lubrication causes inconsistent torque, insufficient preload or bolt overloading.
Packaging is removed in advance for counting. The original sealed package provides rust and dust protection. Once opened, the protection period is greatly shortened and long-term storage is not supported.
Pitting corrosion, rust inside thread roots or surface flaking require direct scrapping. Pitting creates stress concentration points, raising fatigue fracture risk under cyclic loads. Most North American project codes do not allow reusing bolts with pitting.
Only light surface surface tarnish without pits or thread damage, and the original lubricant layer remains intact. Clean the surface properly and reapply rust prevention. Confirm acceptance with the project inspector before use and keep inspection records.
Important note: Do not aggressively wire-brush threads. Thread profile damage will cause assembly failure.
Cleaning shall not alter mechanical properties or thread geometry. Reconditioned bolts are not suitable for slip-critical connections; they can only be considered for static, non-primary load applications.
Keep warehouse dry and ventilated, away from rain and condensation. Separate from chemical and acidic materials. Store on pallets at least 10cm above ground.
Keep unissued bolts in original sealed packaging. Open packages only when needed. Reseal leftover bolts after partial unpacking.
Store A325 separately from oily parts, scraps and other fasteners to avoid cross contamination and thread damage.
Track batch numbers and receiving dates. Ship older stock first to avoid exceeding the anti-rust shelf life.
Incoming inspection: Check package integrity, surface condition and threads for rust, dents or contamination
Regular check: Monitor humidity, package damage and moisture at the bottom of stacks
Issuance control: Open packages only before assembly
Rust judgement: Scrap bolts with pitting or thread rust; consult inspector for light tarnish before reconditioning
Document retention: Keep inventory logs and reconditioning records for inspector review
Q1: Can lightly rusted A325 bolts be cleaned and reused for slip-critical connections? A1: Not recommended. Cleaning changes surface condition and slip coefficient. Reconditioned bolts are not acceptable for slip-critical joints.
Q2: Can A325 bolts contaminated with machine oil be used after cleaning? A2: It depends whether the pre-applied lubricant is dissolved. Damaged lubricant leads to unstable torque, not allowed for high-preload critical connections.
Q3: Do sealed A325 bolts have a shelf life? A3: Factory anti-rust packaging has a limited protection period. Even unopened bolts need visual inspection before use after long storage.