Stainless Steel Fastener Galling: Thread Seizing During Tightening
You are here: Home » News » Industry News » Stainless Steel Fastener Galling: Thread Seizing During Tightening

Stainless Steel Fastener Galling: Thread Seizing During Tightening

Views: 0     Author: TOPBOLT technical team     Publish Time: 2026-11-17      Origin: Site

Inquire

facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
telegram sharing button
sharethis sharing button

1. What is Thread Galling

Galling is adhesive wear, also known as cold welding or thread seizing. Austenitic stainless steel has a thin chromium passive film on the surface. Under high contact pressure and friction during tightening, the passive film breaks. Bare metal asperities contact and bond at molecular level. Further rotation tears the thread surface and transfers material, locking bolt and nut together and making disassembly impossible. Many buyers assume seizing only comes from excessive torque. Even with correct torque control, same-grade stainless steel pairs still suffer galling easily. Galling can happen suddenly after only a few engaged threads.

2. Galling Difference Between 304 and 316 Stainless Steel

Both 304 (A2) and 316 (A4) are austenitic stainless steels with high work-hardening rate and galling risk, while their behaviors differ.

表格

Grade

Galling Tendency

Key Features

Notes

304 / 304L

High

No molybdenum, faster work hardening. Widely used in normal environments. High risk when assembled dry

For indoor and fresh water service. Lubrication required. Avoid repeated assembly of 304 bolt matched with 304 nut

316 / 316L

Moderate to High

Contains molybdenum for better chloride resistance. Slightly lower hardening rate than 304, but galling cannot be eliminated

Coastal, chemical and humid corrosive service. Anti-seize treatment cannot be skipped

3. Risks of Repeated Assembly and Disassembly

Every assembly cycle damages the passive oxide layer and roughens thread flanks. The chance of galling rises after each rework. Fasteners that have galled and been forced apart have permanent thread deformation and shall not be reused. For machinery requiring routine maintenance, anti-galling measures must be specified instead of using carbon steel fastening practices.

4. Lubricant Selection for Anti-Galling

4.1 Anti-Seize Compounds for Different Working Conditions

  • Copper-based anti-seize: General purpose, medium temperature range, cost-effective; not allowed for copper-contamination sensitive applications

  • Nickel-based anti-seize: High temperature service, widely used on hot piping and valve connections

  • PTFE paste / coating: Clean service, food and pharmaceutical equipment, no metallic fillers

  • Molybdenum disulfide grease: Stable medium temperature, not suitable for long-term humid corrosive environments

4.2 Assembly Guidelines

Clean threads before fitting; hand thread engagement first; avoid impact tools with high speed; reduce tightening speed to limit friction heat.

5. Sourcing and Selection Mistakes

Many overseas maintenance buyers only check corrosion grade and ignore galling risk. Same-grade pairs (304 to 304, 316 to 316) carry the highest risk. Mixed-grade pairing can reduce risk but cannot fully prevent seizing.

DIN933 Stainless Steel Hex Bolt

6. Remedial Action for Seized Threads

Do not apply extra torque once galling occurs. Penetrating oil can be applied and left to soak before slow reverse loosening. If failed, destructive cutting or drilling is required. Both bolt and nut shall be scrapped.

7. FAQ

Q1: Does 316 gall less than 304, so anti-seize is unnecessary?

A1: No. 316 only has slightly lower galling tendency. Same-grade 316 pairs still seize easily, especially in corrosive conditions.

Q2: Is galling the same as fusion welding?

A2: It is microscopic cold welding at room temperature, without melting heat input, yet the adhesion can lock the joint completely.

Q3: Can I reuse galled fasteners after grinding threads?

A3: Not recommended. Thread profile is permanently damaged. Reassembly will lead to high risk of repeated galling failure.

Quick Links

Fasteners

Contact Us

WhatsApp: +1 5419089592
Phone: +86 15825577288
Email: sales2@topboltmfg.com
Address: tongtu Road, Yinzhou District, Ningbo, China

Join Our Newsletter

Promotions, new products and sales. Directly to your inbox.
Copyright ©  2024 Ningbo Topbolt Metalworks Co., Ltd. All Rights Reserved. Sitemap. Privacy Policy