Dacromet Fasteners: Repair Solutions for Damaged Dacromet Coating
You are here: Home » News » Industry News » Dacromet Fasteners: Repair Solutions for Damaged Dacromet Coating

Dacromet Fasteners: Repair Solutions for Damaged Dacromet Coating

Views: 0     Author: TOPBOLT technical team     Publish Time: 2026-11-26      Origin: Site

Inquire

facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
telegram sharing button
sharethis sharing button

1. Common Damage Types and Field Repair Availability

Dacromet coating thickness usually ranges from 8μm to 20μm, so scratches and chipping happen easily. Repair permission depends on damage depth, exposed area and load condition.

1.1 Light surface scratches without substrate exposure

Only the top finish is scratched while the zinc-aluminum base layer remains intact. No repair is required. It is merely cosmetic and normally passes inspection.

1.2 Local chipping with bare substrate, small exposed area

The steel base is exposed but the damaged area is limited and not located on threads or high-stress zones. Approved Dacromet touch-up coating can be applied for field repair.

1.3 Large peeling, thread damage or damage on main loaded section

Coating peeling, thread root damage or chipping on the loaded shank are not suitable for field repair. Touch-up coating has weaker adhesion and will peel off under vibration or cyclic load. These fasteners should be re-coated or scrapped.

Threaded areas should be avoided for on-site touch-up. Touch-up paint tends to build up in thread gaps, resulting in go/no-go gauge jamming and unstable preload. For high-temperature high-strength fasteners such as A193 B7, re-coating at factory is the preferred solution once the coating on threads is damaged.

2. Compatibility Comparison of Touch-up Materials vs Original Dacromet

Repair Material

Compatibility with Original Dacromet

Curing Method

Salt Spray Performance After Repair

Application Scope

Dacromet zinc-aluminum touch-up coating

Good, same coating system, stable adhesion

Air dry / low-temperature bake

60%~80% of original salt spray life

Local touch-up for non-thread structural fasteners

Ordinary cold galvanizing spray

Fair, risk of interface separation

Air dry

Fast salt spray decay, white rust along edges

Temporary cosmetic cover only, not for long-term corrosion service

Epoxy zinc-rich paint

Poor, potential galvanic mismatch

Ambient cure

White rust appears at boundary quickly

Not recommended for Dacromet fastener repair

Silver decorative paint

Very poor, no sacrificial protection

Air dry

Red rust occurs in short time

Forbidden for corrosion repair

3. Salt Spray Performance and Degradation Mechanism After Repair

Original Dacromet is cured at high temperature with stacked zinc-aluminum flakes, providing barrier protection plus sacrificial anode protection. Most field repair coatings cure at ambient temperature, so density and bonding strength are lower.

  1. Properly applied matching Dacromet touch-up coating delivers decent corrosion resistance, but rarely fully matches original performance.

  2. The boundary between old and new coating is the weakest spot, where white rust usually starts during salt spray test.

  3. Poor surface preparation with oil, loose rust or residual coating will cause peeling even with high-quality repair paint.

  4. For high-temperature service above 200℃, air-dried touch-up materials will degrade and powder faster than factory Dacromet.

4. Standard Field Repair Procedure

4.1 Surface Preparation

Gently polish damaged zones with 400–600 grit sandpaper or nylon brush to remove loose coating and rust. Polish outward 5–10mm beyond the damaged edge. Clean with alcohol or degreaser and dry completely. Do not apply paint on contaminated surfaces.

4.2 Material Selection and Application

Use zinc-aluminum touch-up paint compatible with original Dacromet. Apply multiple thin coats instead of one heavy coat to avoid pinholes and sagging. Brush application is preferred for small spots to prevent thread clogging.

4.3 Curing

Follow the manufacturer’s curing instruction. Do not stack, rub or assemble before full curing.

4.4 Thickness Check

Use a coating thickness gauge to verify that repaired area reaches thickness close to original specification.

5. Acceptance Criteria for Repaired Dacromet Fasteners

Confirm acceptance rules with supervisors and clients in advance:

  • Acceptable: Small damage area, non-load-critical zone, matching Dacromet touch-up coating, no blistering or lifting.

  • Conditionally accepted: For secondary supporting components, with written repair notes, not for vibrating equipment, high-temperature or pressure-critical connections.

  • Rejected: Thread damage, damage on loaded shank, blistering after repair, non-compatible paint, large peeling area.

FAQ

Q1: Can minor scratches on Dacromet fasteners be left without repair? A1: Shallow scratches that do not expose the steel substrate can generally be accepted without repair. Dacromet has passive self-healing performance, and only cosmetic defects will not shorten the corrosion resistance life.

Q2: Can cold galvanizing spray replace dedicated Dacromet touch-up paint? A2: It is not recommended. Cold galvanizing paint has different formulation system. The interface between old and new coating tends to delaminate, and the salt spray resistance drops significantly, which may lead to inspection failure.

Q3: Is it allowed to repair damaged threads of A193 B7 Dacromet bolts on site? A3: Thread damage is not suitable for on-site touch-up. The repair coating may accumulate on thread profile and cause torque fluctuation. Damaged threaded fasteners should be sent back for re-coating or scrapped.

Quick Links

Fasteners

Contact Us

WhatsApp: +1 5419089592
Phone: +86 15825577288
Email: sales2@topboltmfg.com
Address: tongtu Road, Yinzhou District, Ningbo, China

Join Our Newsletter

Promotions, new products and sales. Directly to your inbox.
Copyright ©  2024 Ningbo Topbolt Metalworks Co., Ltd. All Rights Reserved. Sitemap. Privacy Policy